Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 1.07 kN/m | 6.11 pli | JIS K6301-B |
Stellarchem LP-880 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |