Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tear Strength = 1.07 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 1.07 kN/m
6.11 pli
JIS K6301-B
Stellarchem LP-880 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..