Mechanical Properties Metric English Comments
Tear Strength 10.3 kN/m
59.0 pli
ASTM D624
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7335-1000 TPE
Product Description: StarFlex P 7335-1000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelExcellent ColorabilityGood WeatherabilityFDA and medical grades avai..
Tear Strength 10.3 kN/m
59.0 pli
ASTM D624
STAR Thermoplastic Alloys & Rubbers StarMediflex P 7025-1000 TPE
Product Description: StarMediflex P 7025-1000 is an easy processing TPE designed for injection molding. This particular class of TPE material for medical products and tubing applications. Features:S..
Tear Strength 10.3 kN/m
59.0 pli
ASTM D624
STAR Thermoplastic Alloys & Rubbers StarMediflex P 7035-1000 TPE
Product Description: StarMediflex P 7035-1000 is an easy processing TPE designed for injection molding. This particular class of TPE material for medical products and tubing applications. Features:S..