Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 10.3 kN/m | 59.0 pli | ASTM D624 |
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7335-1000 TPE Product Description: StarFlex P 7335-1000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelExcellent ColorabilityGood WeatherabilityFDA and medical grades avai.. |
|||
Tear Strength | 10.3 kN/m | 59.0 pli | ASTM D624 |
STAR Thermoplastic Alloys & Rubbers StarMediflex P 7025-1000 TPE Product Description: StarMediflex P 7025-1000 is an easy processing TPE designed for injection molding. This particular class of TPE material for medical products and tubing applications. Features:S.. |
|||
Tear Strength | 10.3 kN/m | 59.0 pli | ASTM D624 |
STAR Thermoplastic Alloys & Rubbers StarMediflex P 7035-1000 TPE Product Description: StarMediflex P 7035-1000 is an easy processing TPE designed for injection molding. This particular class of TPE material for medical products and tubing applications. Features:S.. |