Polymer Property : Tear Strength = 520 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 91.1 kN/m
520 pli
Die C, 510 mm/min; ASTM D624
PolyOne Geon™ Vinyl Flexible B4D01 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tear Strength 91.1 kN/m
520 pli
Dow Pellethane® 2102-85A Polyurethane Elastomer, Polyester Polycaprolactone Based  (discontinued **)
PELLETHANE® 2102-85A elastomer is a polyester polycaprolactone based polyurethane elastomer which combines excellent resistance to fuels and oils with enhanced UV stability and good hydrolytic stab..
Tear Strength 91.2 kN/m
520 pli
Die C; ASTM D624
Mearthane Durethaneâ„¢ S DS-685A Solid Polyurethane Elastomer
MDI backbone: ester.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, ..
Tear Strength 91.2 kN/m
520 pli
ASTM D624
Multibase Multi-Flex® D 4701 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good I..
Tear Strength 91.2 kN/m
520 pli
ASTM D624
Multibase Multi-Flex® D 5302 ELF Black TPO Thermoplastic Polyolefin Elastomer
Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Tear Strength 91.2 kN/m
520 pli
ASTM D624
Teknor Apex UNIPRENE® 7010-50D Thermoplastic Elastomer
Information provided by Teknor Apex Company
Tear Strength 91.2 kN/m
520 pli
Die C; ASTM D624
Teknor Apex Telcar® TL-86-K986-A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec..
Tear Strength 91.2 kN/m
520 pli
ASTM D624
Buckeye Polymers BP Flex D5606 TPO
TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. These resins have excellent UV resistance and have a..