Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0080 - 0.012 cm/cm
0.0080 - 0.012 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore D 38
38
15 sec; ASTM D2240
53
53
ASTM D2240
Tensile Strength at Break 20.7 MPa
3000 psi
510 mm/min; ASTM D638
Tensile Strength 13.8 MPa

@Strain 100 %
2000 psi

@Strain 100 %
510 mm/min; ASTM D638
Elongation at Break 340 %
340 %
510 mm/min; ASTM D638
Tear Strength 91.1 kN/m
520 pli
Die C, 510 mm/min; ASTM D624
Compression Set 45 %

@Temperature 23.0 °C,
Time 79200 sec
45 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
Clash Berg Modulus 0.310 GPa

@Temperature -22.0 °C
45.0 ksi

@Temperature -7.60 °F
ASTM D1043
0.614 GPa

@Temperature -35.0 °C
89.1 ksi

@Temperature -31.0 °F
ASTM D1043
Thermal Properties Metric English Comments
Brittleness Temperature -27.0 °C
-16.6 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 179 - 185 °C
354 - 365 °F
196 - 207 °C
385 - 405 °F
Descriptive Properties Value Comments
Appearance Opaque
Features High Gloss
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion
Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America