Mechanical Properties Metric English Comments
Tear Strength 73.0 - 88.0 kN/m
417 - 502 pli
NF EN ISO 1421
Isoflon Tisoflon® 10K Polytetrafluoroethylene Coated Kevlar Fabric
PTFE coated Kevlar fabric TISOFLON®Information provided by Isoflon.