Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 5.30 kN/m | 30.2 pli | Trouser, Press-cured 5 minutes at 190°C; DIN 53508 |
DuPont Vamac® DP DIAK No. 7 Coagent Test Compound Vamac® DP is an ethylene acrylic dipolymer elastomer. Its general performance characteristics are similar to those of the Vamac® terpolymers, including:Good oil and chemical resistanceHigh temper.. |