Polymer Property : Tear Strength = 30.2 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 5.30 kN/m
30.2 pli
Trouser, Press-cured 5 minutes at 190°C; DIN 53508
DuPont Vamac® DP DIAK No. 7 Coagent Test Compound
Vamac® DP is an ethylene acrylic dipolymer elastomer. Its general performance characteristics are similar to those of the Vamac® terpolymers, including:Good oil and chemical resistanceHigh temper..