Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 0.900 kN/m | 5.14 pli | Typical; ASTM D264-91 Die C |
Rogers Corporation Poron® 4790-92-15 Urethane Foam, Extra Soft, Slow Rebound Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression .. |
|||
Tear Strength | >= 0.900 kN/m | >= 5.14 pli | ASTM D642-91 Die C |
Rogers Corporation Poron® Shock Seal™ 4790-79-12 Urethane Foam, Industrial Grade Thickness: 0.080"- 0.375"Color: BlackInformation provided by Rogers Corporation. |
|||
Tear Strength | >= 0.900 kN/m | >= 5.14 pli | ASTM D624, Die C |
Rogers Corporation R/bak® SS Cushion Mounting Materials, Supported Soft R/bak materials are high-density, open cell, polyurethane foams used to build thickness on the cylinder, provide cushioning and absorb vibration in the Flexographic printing process. The use of R/b.. |
|||
Tear Strength | >= 0.900 kN/m | >= 5.14 pli | Die C; ASTM D624 |
Rogers Corporation Poron® 4701-40-20 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |