Mechanical Properties Metric English Comments
Tear Strength 0.900 kN/m
5.14 pli
Typical; ASTM D264-91 Die C
Rogers Corporation Poron® 4790-92-15 Urethane Foam, Extra Soft, Slow Rebound
Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression ..
Tear Strength >= 0.900 kN/m
>= 5.14 pli
ASTM D642-91 Die C
Rogers Corporation Poron® Shock Seal™ 4790-79-12 Urethane Foam, Industrial Grade
Thickness: 0.080"- 0.375"Color: BlackInformation provided by Rogers Corporation.
Tear Strength >= 0.900 kN/m
>= 5.14 pli
ASTM D624, Die C
Rogers Corporation R/bak® SS Cushion Mounting Materials, Supported Soft
R/bak materials are high-density, open cell, polyurethane foams used to build thickness on the cylinder, provide cushioning and absorb vibration in the Flexographic printing process. The use of R/b..
Tear Strength >= 0.900 kN/m
>= 5.14 pli
Die C; ASTM D624
Rogers Corporation Poron® 4701-40-20 Cellular Urethane Foam
Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h..