Polymer Property : Tear Strength = 49.9 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 49.9 kN/m
285 pli
ASTM D624
Multibase Multi-Flex® TPE D 4201 BLK
Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Tear Strength 49.9 kN/m
285 pli
Die C
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 60 PHR Dixie Clay Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tear Strength 49.9 - 58.6 kN/m
285 - 335 pli
ASTM D624
3M 32661 Heavy Duty Performance Coating - Part B
3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and ..
Tear Strength 49.9 - 58.6 kN/m
285 - 335 pli
ASTM D624
3M 32662 Black Heavy Duty Performance Coating - Part B
3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and ..
Tear Strength 49.9 - 58.6 kN/m
285 - 335 pli
ASTM D624
3M 32660 Heavy Duty Performance Coating - Part A
3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and ..
Tear Strength 49.9 - 58.6 kN/m
285 - 335 pli
ASTM D624
3M 32665 Green Heavy Duty Performance Coating - Part B
3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and ..
Tear Strength 49.9 - 58.6 kN/m
285 - 335 pli
ASTM D624
3M 32666 Tan Heavy Duty Performance Coating - Part B
3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and ..
Tear Strength 49.9 kN/m
285 pli
Die C
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 60 PHR Dixie Clay Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tear Strength 49.9 - 58.6 kN/m
285 - 335 pli
ASTM D624
3M 32663 Medium Grey Heavy Duty Performance Coating - Part B
3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and ..
Tear Strength 49.9 - 58.6 kN/m
285 - 335 pli
ASTM D624
3M 32664 Light Gray Heavy Duty Performance Coating - Part B
3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and ..