Multibase Multi-Flex® TPE D 4201 BLK

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Multibase
Trade Name Multi-Flex® TPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPE D 4201 BLK.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
ASTM D792
Melt Flow 1.0 g/10 min
1.0 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore D 34
34
10 sec; ASTM D-2240
Tensile Strength, Ultimate 8.30 MPa
1200 psi
ASTM D412
Elongation at Break 560 %
560 %
ASTM D412
Flexural Modulus 0.207 GPa
30.0 ksi
method 1, Proc.B; ASTM D-790
Tear Strength 49.9 kN/m
285 pli
ASTM D624