Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 80.6 kN/m | 460 pli | ASTM D624 (Die C) |
Lubrizol Advanced Materials PEARLTHANE® 16N80 Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® 16N80 is a polyether-based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mechanical properties and excellent hydrolys.. |
|||
Tear Strength | 80.6 kN/m | 460 pli | ASTM D624 (Die C) |
Lubrizol Advanced Materials PEARLTHANE® 12K85LB Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® 12K85 LB is a standard polyester-based TPU with a lubricating additive, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mech.. |
|||
Tear Strength | 80.6 kN/m | 460 pli | ASTM D624 |
Huntsman IROGRAN® A 85 P 4380 TPU-Polyether Introduction: IROGRAN A 85 P 4380 is a flame-retardant, halogen-free, thermoplastic polyether-polyurethane intended for extrusion and injection molding applications. Additional characteristics of th.. |
|||
Tear Strength | 80.6 kN/m | 460 pli | Injection molded parts; ASTM D624 |
Huntsman IROGRAN® CA116-203 TPU-Polyester Introduction: IROGRAN CA116-203 is a high performance polyester based thermoplastic polyurethane intended for flat die extrusion applications. IROGRAN CA116-203 is part of the HUNTSMAN film and shee.. |
|||
Tear Strength | 80.6 kN/m | 460 pli | Injection molded parts; ASTM D624 |
Huntsman IROGRAN® CA116-205 TPU-Polyester Introduction: IROGRAN CA116-205 is a high performance polyester based thermoplastic polyurethane intended for flat die extrusion applications. IROGRAN CA116-205 is part of the HUNTSMAN film and shee.. |
|||
Tear Strength | 80.6 kN/m | 460 pli | Injection molded parts; ASTM D624 |
Huntsman IROGRAN® A 92 E 4670 TPU-Polyester Introduction IROGRAN A 92 E 4670 is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion/injection molding product range and offers a spe.. |
|||
Tear Strength | 80.6 kN/m | 460 pli | ASTM D624 (Die C) |
Lubrizol Advanced Materials PEARLTHANE® Clear 15N80 Thermoplastic Polyurethane Elastomer PEARLTHANE® CLEAR 15N80 is a polyether copolymer-based TPU, supplied in form of translucent, colorless, combining low hardness with excellent mechanical properties and excellent hydrolysis resist.. |
|||
Tear Strength | 80.7 kN/m | 460 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR N220 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 80.6 kN/m | 460 pli | ISO 34-1 |
Alliance Polymers Viprene™ G50A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G50A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tear Strength | 80.6 kN/m | 460 pli | ISO 34-1 |
Alliance Polymers Viprene™ G50A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G50A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tear Strength | 80.6 kN/m | 460 pli | ASTM D412 |
ACC EP EF EPI Engineered Polymers Extra Flex Polyurea EP EF, Extra Flex Polyurea, “Powered by Reactamine® Technology, is a two component 100% solid Polyurea, with superior performance in industrial applications. EP EF displays extremely fast cure tim.. |
|||
Tear Strength | 80.6 kN/m | 460 pli | ASTM D412 |
ACC SMP™ EP EF SP EPI Engineered Polymers Extra Flex with Silicone EP EF SP, “Powered by Reactamine® Technology”, is a two component 100% solid Silicone Polyurea with superior performance in industrial applications. EP EF SP displays extremely fast cure times wi.. |
|||
Tear Strength | 80.7 kN/m | 460 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR N220 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 80.6 kN/m | 460 pli | Die C; ASTM D624 |
Lubrizol Estane® 2103-80AEF Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Film resin for injection blow moldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product l.. |