Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 79.7 kN/m | 455 pli | Die C, 2 in/min; ASTM D1004 |
PolyOne Geon™ Vinyl Flexible B85UB Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 79.8 kN/m | 455 pli | ISO 34-1B |
Lubrizol Advanced Materials PEARLTHANE® 11T80 Thermoplastic Polyurethane Elastomer Type : Pearlthane® 11T80 is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining hardness with excellent mechanical pr.. |