Polymer Property : Tear Strength = 44.4 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 44.4 kN/m
253 pli
post cured- 4 hours at 177°C; Die B
Multibase SILASTIC® Q7-4750 Dow-Corning Biomedical Grade ETR Elastomer
Information provided by Multibase
Tear Strength 44.4 kN/m
253 pli
Dow Corning SILASTIC® LC-50-2004 PART A&B KIT
50 Durometer, 2 parts, 1 to 1 mix, translucent, injection molding grade Liquid Silicone Rubber. Fast curing speed, long pot life (72 hours), high transparency, high tear strength, low compression se..