Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 44.4 kN/m | 253 pli | post cured- 4 hours at 177°C; Die B |
Multibase SILASTIC® Q7-4750 Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tear Strength | 44.4 kN/m | 253 pli | |
Dow Corning SILASTIC® LC-50-2004 PART A&B KIT 50 Durometer, 2 parts, 1 to 1 mix, translucent, injection molding grade Liquid Silicone Rubber. Fast curing speed, long pot life (72 hours), high transparency, high tear strength, low compression se.. |
|||
Tear Strength | 44.3 kN/m | 253 pli | 44.3 kN/m at 23°C. Value at 100°C is 18.4 kN/m. TPE-0056 (ASTM D 624) |
Advanced Elastomer Systems Santoprene® 251-92 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can b.. |