Polymer Property : Tear Strength = 44.0 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 44.0 kN/m
251 pli
Die C
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 1.0 PHR MBT
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tear Strength 44.0 kN/m
251 pli
Die B
Momentive Performance Materials Siloprenâ„¢ CLS 5000 Liquid Silicone Rubber - Self-Bonding / Customized
This LSR elastomer is a self-bonding, customized, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate..
Tear Strength 44.0 kN/m
251 pli
Die B
Momentive Performance Materials Siloprenâ„¢ LSR 2670FC High Productivity Liquid Silicone Rubber
This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera..
Tear Strength 44.0 kN/m
251 pli
Die C
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 1.0 PHR MBT
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tear Strength 44.0 kN/m
251 pli
ASTM D624
UBE UBEPOL BR150B Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE.
Tear Strength 44.0 kN/m
251 pli
Die C; ASTM D624
Lubrizol Estane® 58201 Thermoplastic Polyurethane
Type: Estane® 58201 is an 82A Polyether-type thermoplastic polyurethane (TPU) compound.Features: Tear resistant properties.Uses: Injection Molding and general extrusion techniques.Available in Euro..
Tear Strength 44.0 kN/m
251 pli
ASTM D 624
API Megol AM DP2268/65PA12 SEBS Adhesion Modified Overmolding for PA
Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as ..
Tear Strength 44.0 kN/m
251 pli
ISO 34-B
AlphaGary Evoprene™ G 927 SEBS Thermoplastic Elastomer
Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi..