Polymer Property : Tear Strength = 4.60 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 0.806 kN/m

@Thickness 3.05 mm
4.60 pli

@Thickness 0.120 in
Zircar Ceramics APA-1 Alumina Paper
ZIRCAR Alumina Papers are uniform structures made principally of alumina fiber. APA-1 is a strong, flexible material with fibers held together with organic binder that is available in roll or sheet..