Mechanical Properties Metric English Comments
Tear Strength 0.800 kN/m
4.56 pli
Fujipoly Industries Sarcon® 85T Thin-Film TR
Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of ..
Tear Strength 0.800 kN/m
4.56 pli
BS EN ISO 8067 1995
Zotefoams Plastazote® LD50CN Conductive Low Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..