Mechanical Properties Metric English Comments
Tear Strength 39.9 kN/m
228 pli
Die C
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.0 PHR MBT
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Tear Strength 39.9 kN/m
228 pli
Die C
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR N330 (HAF) Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Tear Strength 39.9 kN/m
228 pli
Die C
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.0 PHR MBT
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Tear Strength 39.9 kN/m
228 pli
Die C
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR N330 (HAF) Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..