Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | >= 38.53 kN/m | >= 219.9 pli | ASTM D624 |
Multibase Multi-Flex® TPE A 7606 GRAPHITE The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tear Strength | >= 38.53 kN/m | >= 219.9 pli | ASTM D624 |
Multibase Multi-Flex® TPE A 7606 JA6A BLK The burn rate is 1.2 in/min (30 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tear Strength | >= 38.53 kN/m | >= 219.9 pli | ASTM D624 |
Multibase Multi-Flex® TPE A 7606 UV NAT The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |