Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 37.9 kN/m | 216 pli | Die B,post cured- 2 hours at 177°C; ASTM D624 |
Multibase C6-135 Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 37.9 kN/m | 216 pli | Die B, no post cure; ASTM D624 |
Multibase C6-350 LH Parts A and B Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 37.9 kN/m | 216 pli | |
Dow Corning SILASTIC® LS 5-8754 FLUOROSILICONE BASE 50 Durometer, off-white, molding grade fluorosilicone base.Information provided by Dow Corning |