Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 34.0 kN/m | 194 pli | ISO 34-1 |
PolyOne OnFlex™ S FR 80A-3S1892 Thermoplastic Elastomer (TPE) OnFlex™-S FR thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially flame retarded with a highly effective, RoHS compliant halo.. |
|||
Tear Strength | 34.0 kN/m | 194 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ CLS 8150 Liquid Silicone Rubber - Self-Bonding / Customized This LSR elastomer is a self-bonding, customized, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Tear Strength | 34.0 kN/m | 194 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 2725/40 Liquid Silicone Rubber - Self-Bonding / Self-Lubricating This LSR elastomer is a self-bonding, self-lubricating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at e.. |
|||
Tear Strength | 34.0 kN/m | 194 pli | ISO 34/1 |
A. Schulman INVISION™ VX-5075UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5075UI is a polyolefin-based thermoplastic of 75 Shore A durometer, which has been formulated for soft touch, mar resistance, low gloss, and excellent weatherability. Appli.. |
|||
Tear Strength | 34.0 kN/m | 194 pli | Die C, at 23°C |
DuPont Vamac® GLS Sample Compound Vulcanizate Slab Cured Test slab is press cured for 5 minutes at 177°C and post cured for 4hrs at 175°C. Vulcanizate performance test data can help end-users evaluate the potential fitness of similar compounds for thei.. |
|||
Tear Strength | 34.0 kN/m | 194 pli | ISO 34/1 |
A. Schulman INVISION™ VX-5075UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5075UI is a polyolefin-based thermoplastic of 75 Shore A durometer, which has been formulated for soft touch, mar resistance, low gloss, and excellent weatherability. Appli.. |
|||
Tear Strength | 34.0 kN/m | 194 pli | ISO 34/1 |
A. Schulman INVISION™ VX-5075UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5075UI is a polyolefin-based thermoplastic of 75 Shore A durometer, which has been formulated for soft touch, mar resistance, low gloss, and excellent weatherability. Appli.. |
|||
Tear Strength | 34.0 kN/m | 194 pli | ISO 34/1 |
A. Schulman INVISION™ VX-5075UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5075UI is a polyolefin-based thermoplastic of 75 Shore A durometer, which has been formulated for soft touch, mar resistance, low gloss, and excellent weatherability. Appli.. |
|||
Tear Strength | 34.0 kN/m | 194 pli | ISO 34/1 |
A. Schulman INVISION™ VX-5075UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5075UI is a polyolefin-based thermoplastic of 75 Shore A durometer, which has been formulated for soft touch, mar resistance, low gloss, and excellent weatherability. Appli.. |
|||
Tear Strength | 34.0 kN/m | 194 pli | with incision; ISO 34B |
Lubrizol ESTANE® GP65AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 65AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Tear Strength | 34.0 kN/m | 194 pli | ISO 34/1 |
A. Schulman INVISION™ VX-5075UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5075UI is a polyolefin-based thermoplastic of 75 Shore A durometer, which has been formulated for soft touch, mar resistance, low gloss, and excellent weatherability. Appli.. |
|||
Tear Strength | 34.0 kN/m | 194 pli | |
Dow Corning SILASTIC® 24020-V NATURAL SILICONE RUBBER 70 Durometer, natural, peroxide cured, molding grade Silicone Rubber Compound.Information provided by Dow Corning |
|||
Tear Strength | 34.0 kN/m | 194 pli | M.D., Split Tear @ 254 mm/min; ASTM D1938 |
Eastman Embrace LV Copolyester for Extruded/Cast Film Applications:Beverage packagingDairy packagingFood packagingJuice packagingPharmaceutical packagingSoft drink packagingKey Attributes:Customizable shrink curveEye-catching 360° graphic capabilityLo.. |
|||
Tear Strength | 34.0 kN/m | 194 pli | 73°C, Die C; ASTM D624 |
ExxonMobil Geolast® 701-87W183 Thermoplastic Elastomer A hard, black, oil resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good hot air and hot oil resistance for use in a wide range of applic.. |
|||
Tear Strength | 34.0 kN/m | 194 pli | Perpendicular to flow; ISO 34-B |
AlphaGary Evoprene™ GF 6256 Automotive Thermoplastic Elastomer Evoprene™ GF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab.. |
|||
Tear Strength | 34.0 kN/m | 194 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® RT-3780 Thermoplastic Elastomer - SBC, Mineral Filled
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledNaturalApplications:General PurposeMarket:Consumer GoodsIndustrialBuilding and ConstructionProcessing Method:Injection Molding.. |
|||
Tear Strength | 34.0 kN/m | 194 pli | Type C; ASTM D624 |
LG Chemical LC175 Polyolefin Elastomer for Polymer Modification Features: Improved impact strength in polypropylene; Excellent filler acceptance; Available as pellet form; Outstanding toughness with flexible performance; and Reduction of product weightApplicatio.. |