Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 34.0 kN/m
194 pli
ISO 34-1
PolyOne OnFlex™ S FR 80A-3S1892 Thermoplastic Elastomer (TPE)
OnFlex™-S FR thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially flame retarded with a highly effective, RoHS compliant halo..
Tear Strength 34.0 kN/m
194 pli
Die B
Momentive Performance Materials Siloprenâ„¢ CLS 8150 Liquid Silicone Rubber - Self-Bonding / Customized
This LSR elastomer is a self-bonding, customized, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate..
Tear Strength 34.0 kN/m
194 pli
Die B
Momentive Performance Materials Siloprenâ„¢ LSR 2725/40 Liquid Silicone Rubber - Self-Bonding / Self-Lubricating
This LSR elastomer is a self-bonding, self-lubricating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at e..
Tear Strength 34.0 kN/m
194 pli
ISO 34/1
A. Schulman INVISION™ VX-5075UI Soft Touch Polyolefin Thermoplastic
DescriptionInvision™ VX-5075UI is a polyolefin-based thermoplastic of 75 Shore A durometer, which has been formulated for soft touch, mar resistance, low gloss, and excellent weatherability. Appli..
Tear Strength 34.0 kN/m
194 pli
Die C, at 23°C
DuPont Vamac® GLS Sample Compound Vulcanizate Slab Cured
Test slab is press cured for 5 minutes at 177°C and post cured for 4hrs at 175°C. Vulcanizate performance test data can help end-users evaluate the potential fitness of similar compounds for thei..
Tear Strength 34.0 kN/m
194 pli
ISO 34/1
A. Schulman INVISION™ VX-5075UI Soft Touch Polyolefin Thermoplastic
DescriptionInvision™ VX-5075UI is a polyolefin-based thermoplastic of 75 Shore A durometer, which has been formulated for soft touch, mar resistance, low gloss, and excellent weatherability. Appli..
Tear Strength 34.0 kN/m
194 pli
ISO 34/1
A. Schulman INVISION™ VX-5075UI Soft Touch Polyolefin Thermoplastic
DescriptionInvision™ VX-5075UI is a polyolefin-based thermoplastic of 75 Shore A durometer, which has been formulated for soft touch, mar resistance, low gloss, and excellent weatherability. Appli..
Tear Strength 34.0 kN/m
194 pli
ISO 34/1
A. Schulman INVISION™ VX-5075UI Soft Touch Polyolefin Thermoplastic
DescriptionInvision™ VX-5075UI is a polyolefin-based thermoplastic of 75 Shore A durometer, which has been formulated for soft touch, mar resistance, low gloss, and excellent weatherability. Appli..
Tear Strength 34.0 kN/m
194 pli
ISO 34/1
A. Schulman INVISION™ VX-5075UI Soft Touch Polyolefin Thermoplastic
DescriptionInvision™ VX-5075UI is a polyolefin-based thermoplastic of 75 Shore A durometer, which has been formulated for soft touch, mar resistance, low gloss, and excellent weatherability. Appli..
Tear Strength 34.0 kN/m
194 pli
with incision; ISO 34B
Lubrizol ESTANE® GP65AE Ester Based Thermoplastic Polyurethane
Type: Estane® GP 65AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..
Tear Strength 34.0 kN/m
194 pli
ISO 34/1
A. Schulman INVISION™ VX-5075UI Soft Touch Polyolefin Thermoplastic
DescriptionInvision™ VX-5075UI is a polyolefin-based thermoplastic of 75 Shore A durometer, which has been formulated for soft touch, mar resistance, low gloss, and excellent weatherability. Appli..
Tear Strength 34.0 kN/m
194 pli
Dow Corning SILASTIC® 24020-V NATURAL SILICONE RUBBER
70 Durometer, natural, peroxide cured, molding grade Silicone Rubber Compound.Information provided by Dow Corning
Tear Strength 34.0 kN/m
194 pli
M.D., Split Tear @ 254 mm/min; ASTM D1938
Eastman Embrace LV Copolyester for Extruded/Cast Film
Applications:Beverage packagingDairy packagingFood packagingJuice packagingPharmaceutical packagingSoft drink packagingKey Attributes:Customizable shrink curveEye-catching 360° graphic capabilityLo..
Tear Strength 34.0 kN/m
194 pli
73°C, Die C; ASTM D624
ExxonMobil Geolast® 701-87W183 Thermoplastic Elastomer
A hard, black, oil resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good hot air and hot oil resistance for use in a wide range of applic..
Tear Strength 34.0 kN/m
194 pli
Perpendicular to flow; ISO 34-B
AlphaGary Evoprene™ GF 6256 Automotive Thermoplastic Elastomer
Evoprene™ GF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab..
Tear Strength 34.0 kN/m
194 pli
Die C (graves), 20 in/min; ASTM D624
PolyOne Synprene® RT-3780 Thermoplastic Elastomer - SBC, Mineral Filled  (discontinued **)
Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledNaturalApplications:General PurposeMarket:Consumer GoodsIndustrialBuilding and ConstructionProcessing Method:Injection Molding..
Tear Strength 34.0 kN/m
194 pli
Type C; ASTM D624
LG Chemical LC175 Polyolefin Elastomer for Polymer Modification
Features: Improved impact strength in polypropylene; Excellent filler acceptance; Available as pellet form; Outstanding toughness with flexible performance; and Reduction of product weightApplicatio..