Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 58.8 kN/m | 336 pli | Die C; ASTM D624 |
Lubrizol Estane® T460A Thermoplastic Polyurethane Type: Estane® T460A is a Shore 66A, polyester grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provided b.. |
|||
Tear Strength | 58.8 kN/m | 336 pli | Die C; ASTM D624 |
Lubrizol Estane® T465A Thermoplastic Polyurethane Type: Estane® T465A is a Shore 71A, polyester grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Information Provided by The Lubrizol Cor.. |
|||
Tear Strength | 58.8 kN/m | 336 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.5 PHR Sulfur Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and man.. |
|||
Tear Strength | 58.8 kN/m | 336 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.5 PHR Sulfur Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and man.. |