Polymer Property : Tear Strength = 3.30 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength >= 3.30 kN/m
>= 18.8 pli
Die C; ASTM D624
Rogers Corporation Poron® 4701-60-30 Cellular Urethane Foam
Standard color is black (04); others are available. Passes flammability test MVSS 302. Passes fogging test SAE-J 1736 for 3 hrs. at 100°C (212°F). Passes cold flexibility per MIL-P-12420D at -4..
Tear Strength 3.30 kN/m
18.8 pli
ISO 34-C
Premix Thermoplastics PRESEAL® TPE 6070
PRESEAL TPE 6070 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasketing and grounding applications. Conductivity is achieved with a silver coated glass sp..