Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | >= 3.30 kN/m | >= 18.8 pli | Die C; ASTM D624 |
Rogers Corporation Poron® 4701-60-30 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability test MVSS 302. Passes fogging test SAE-J 1736 for 3 hrs. at 100°C (212°F). Passes cold flexibility per MIL-P-12420D at -4.. |
|||
Tear Strength | 3.30 kN/m | 18.8 pli | ISO 34-C |
Premix Thermoplastics PRESEAL® TPE 6070 PRESEAL TPE 6070 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasketing and grounding applications. Conductivity is achieved with a silver coated glass sp.. |