Mechanical Properties Metric English Comments
Tear Strength 44.7 kN/m
255 pli
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Non-Black, Aerosil 200
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Tear Strength 44.7 kN/m
255 pli
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Non-Black, Aerosil 200
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Tear Strength 44.7 kN/m
255 pli
Dow Corning C6-550 LIQUID SILICONE RUBBER KIT
Dow Corning® Class VI Elastomers are heat cured elastomer raw materials for use by customers fabricating medical devices and parts.Information provided by Dow Corning
Tear Strength 44.7 kN/m
255 pli
Die B, no post cure; ASTM D624
Multibase C6-550 Dow-Corning Class VI Elastomer