Mechanical Properties Metric English Comments
Tear Strength 38.2 kN/m
218 pli
ASTM D412
Stellarchem SV-B75E TPV Compound
This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on ..
Tear Strength 38.2 kN/m
218 pli
Die B; DBPH Cure
Shin-Etsu Silicones KE-5551U High Strength Silicone Elastomer
ShinEtsu KE5551 U is a nominal 50 Durometer base which offers high tensile and tear strengths. Its excellent processing characteristics make it suitable for molding, extrusion and calendaringProduct..
Tear Strength 38.2 kN/m
218 pli
Warp, Breaking Strength w/o Sizing
3M Nextel™ AF-10 Aerospace Woven Fabric 312
Information provided by 3M
Tear Strength 38.2 kN/m
218 pli
Fill, Breaking Strength w/o Sizing
3M Nextel™ AF-10 Aerospace Woven Fabric 312
Information provided by 3M
Tear Strength 38.2 kN/m
218 pli
Warp, Breaking Strength w/o Sizing
3M Nextel™ AF-12 Aerospace Woven Fabric 312
Information provided by 3M
Tear Strength 38.2 kN/m
218 pli
Fill, Breaking Strength w/o Sizing
3M Nextel™ AF-12 Aerospace Woven Fabric 312
Information provided by 3M
Tear Strength 38.2 kN/m
218 pli
Fill, Breaking Strength w/o Sizing
3M Nextel™ BF-20 Woven Fabric 440
Information provided by 3M