Mechanical Properties Metric English Comments
Tear Strength 0.350 kN/m
2.00 pli
ASTM D 624
Eurofoam Evacell EVA 50/S EVA + NR Foam
Foamed polyethylene charged with EVA, with extremely fine cells, excellent elasticity, resilience and mechanical resistance. It can be thermoformed several times. It has completely closed cells, di..
Tear Strength 0.350 kN/m
2.00 pli
ASTM D 624
Eurofoam Porocell POR 304 CM-HD EPDM Foam
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.