Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 0.350 kN/m | 2.00 pli | ASTM D 624 |
Eurofoam Evacell EVA 50/S EVA + NR Foam Foamed polyethylene charged with EVA, with extremely fine cells, excellent elasticity, resilience and mechanical resistance. It can be thermoformed several times. It has completely closed cells, di.. |
|||
Tear Strength | 0.350 kN/m | 2.00 pli | ASTM D 624 |
Eurofoam Porocell POR 304 CM-HD EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |