Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 128 kN/m | 730 pli | Die C; ASTM D624 |
Mearthane Durethaneâ„¢ S DS-450D Solid Polyurethane Elastomer TDI backbone: ester.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, .. |
|||
Tear Strength | 128 kN/m | 730 pli | without incision; ISO 34B |
Lubrizol ESTANE® GP92AT Ether Based Thermoplastic Polyurethane Type: Estane® GP 92AT is an aromatic polyether-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Tear Strength | 128 kN/m | 730 pli | ISO 34 |
Chengdu Polyster FH7560 Thermoplastic Polyether-ester Elastomer (TPEE) Blend of H7560 and self-made flame retardant material. Flame retardant, high tear resistance. Applications requiring flame retardancy, such as wires, cables and optical fiber.Information provided by.. |