Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 22.1 kN/m | 126 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Synprene™ RT-5155 RoHS Natural Styrene Butadiene Block Copolymer (SBC) Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom.. |
|||
Tear Strength | 22.0 kN/m | 126 pli | Die B |
Momentive Performance Materials Silplusâ„¢ 80 MP Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 22.0 kN/m | 126 pli | Die B |
Momentive Performance Materials TSE 221-4U Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 22.0 kN/m | 126 pli | Die B |
Momentive Performance Materials TUFELâ„¢ II 94205 Low Volatile Extrusion Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 22.0 kN/m | 126 pli | Die B |
Momentive Performance Materials TUFELâ„¢ II 94206 Low Volatile Extrusion Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 22.0 kN/m | 126 pli | ASTM D624 |
Multibase Multi-Flex® TPE A 5501 LC GREY Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tear Strength | 22.0 kN/m | 126 pli | Die C; Cross direction; ASTM D624 |
Teknor Apex Sarlink® 4155 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4155 is a low hardness grade possessing exceptional tensile strength, superior compression set, chemical re.. |
|||
Tear Strength | 22.0 kN/m | 126 pli | ASTM D624 |
Teknor Apex Sarlink® 4370 Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4370 is a flame retardant, soft hardness grade exhibiting exceptional chemical resistance, compression set.. |
|||
Tear Strength | 22.0 kN/m | 126 pli | Die C; Cross direction; ASTM D624 |
Teknor Apex Sarlink® 4455 Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4455 is a low hardness grade possessing exceptional tensile strength, superior compression s.. |
|||
Tear Strength | 22.0 kN/m | 126 pli | Method C; ISO 34 |
ELASTO UK Dryflex® 3004-111 TPE, Modified Injection Molding Grade for Auto Interior Parts The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 3004-111 is specifically designe.. |
|||
Tear Strength | 22.0 kN/m | 126 pli | Method C; ISO 34 |
ELASTO UK Dryflex® 3006-101 TPE, Modified Injection Molding Grade for Auto Interior Parts The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 3006-101 is specifically designe.. |
|||
Tear Strength | 22.0 kN/m | 126 pli | ASTM D624 |
ELASTO UK Dryflex® 500500S SEBS Based Material, Unfilled Qualities, 50A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Tear Strength | 22.0 kN/m | 126 pli | ASTM D624 |
ELASTO UK Dryflex® 502500S SEBS Based Material, Unfilled Qualities, 50A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Tear Strength | 22.0 kN/m | 126 pli | ASTM D624 |
ELASTO UK Dryflex® 660550S SEBS Based Material, Semi-Filled Qualities, 55A Hardness, Natural The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Tear Strength | 22.0 kN/m | 126 pli | ASTM D624 |
ELASTO UK Dryflex® 660600S SEBS Based Material, Semi-Filled Qualities, 60A Hardness, Natural The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Tear Strength | 22.0 kN/m | 126 pli | ASTM D624 |
ELASTO UK Dryflex® 662550S SEBS Based Material, Semi-Filled Qualities, 55A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Tear Strength | 22.0 kN/m | 126 pli | ASTM D624 |
ELASTO UK Dryflex® 662600S SEBS Based Material, Semi-Filled Qualities, 60A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Tear Strength | 22.1 kN/m | 126 pli | Die C, Vulcanizate, Press cured, TC95 +3min at 180°C |
Dow Nordel® IP 4570 Heat Resistant Peroxide Compound FormulationNordel® IP 4570 |
|||
Tear Strength | 22.1 kN/m | 126 pli | ASTM D624 |
Aearo E-A-R Specialty Composites VersaDamp™ V-2775 TPE VersaDamp TPEs are olefinic dynamic vulcanizates. The VersaDamp 2000 series materials provide predictable damping performance throughout a broad range of temperatures. They can be injection molded.. |
|||
Tear Strength | 22.0 kN/m | 126 pli | Parallel to flow; ISO 34-B |
AlphaGary Evoprene™ LF 6152 Automotive Thermoplastic Elastomer Evoprene™ LF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab.. |
|||
Tear Strength | 22.0 kN/m | 126 pli | |
ACC MMAD25 Addition Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: cures at room temperature, low viscosity, low shrinkage, high tear and tensile strengths. Applications: plaster casti.. |
|||
Tear Strength | 22.0 kN/m | 126 pli | |
ACC QMSkin 30 Specialist Molding 2-Part Condensation Cure Part of the Amber Chemical Group. Data provided by manufacturer. |