Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 63.7 - 103 kN/m | 364 - 588 pli | |
Taiwan PU Corporation PTMG CPU-42L Polyurethane Casting Elastomer A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, cu.. |