Polymer Property : Tear Strength = 1010 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 177 kN/m
1010 pli
ASTM D624
Kolon ELLAS K-260D Thermoplastic Polyurethane
ApplicationsExtrusion: Antenna, Heel TipInjection: Hose, Tube, SheetIndustry Parts Information provided by API-Kolon.
Tear Strength 177 kN/m
1010 pli
Initial Tear Strength; ASTM D-1004
Saint-Gobain Norton® ECTFE Fluoropolymer Film
Features/Benefits:Outstanding release propertiesPerformance from -200°C (-328°F) to 165°C (330°F)High dielectric strengthExcellent chemical, radiation, weather and abrasion resistanceNon..
Tear Strength 177 kN/m
1010 pli
Die C; ASTM D624
SK Chemicals SKYTHANE® 198A S series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Tear Strength 177 kN/m
1010 pli
Die C; ASTM D624
SK Chemicals SKYTHANE® S198A Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Tear Strength 177 kN/m
1010 pli
Die C; ASTM D624
Lubrizol Estane® S198A Thermoplastic Polyurethane
Type: Estane® S198A is a Shore 98A, polyester grade thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Americas, Europe, Middle East, ..
Tear Strength 177 kN/m
1010 pli
ASTM D624
Toyobo PELPRENE™ P150B Polyester TPE
Features: Polyester TPEInformation provided by Toyobo.
Tear Strength 177 kN/m
1010 pli
Unnicked; ISO 34-1B
Lubrizol Estane® GP 58 DT Thermoplastic Polyurethane
Type: Estane® GP 58DT is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: Translucent spherical pellets.Uses: Injection molding parts, animal identification tagsAvailable in E..
Tear Strength 177 kN/m
1010 pli
ASTM D624
Toyobo A3064D Thermoplastic Polyurethane Elastomer, Injection Grade
Polyether type, featuring excellent resistance to hot water and fungus. Various grades of Toyobo polyurethane TPEs are used in auto parts, hoses, tubes, sporting goods, shoe soles, etc.Information ..