Polymer Property : Modulus of Rupture = 4.35 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Rupture 0.0300 GPa

@Temperature 1370 °C
4.35 ksi

@Temperature 2500 °F
Pyrotek Pyrocast PT-190 Refractory Cast Parts
Pyrocast PT-190 is an extremely dense alumina based refractory. It is best suited for applications where high velocity metal erosion potential is a problem, due to its strength and abrasion resista..
Modulus of Rupture 0.0300 GPa

@Temperature 1370 °C
4.35 ksi

@Temperature 2500 °F
Pyrotek Pyrocast SC-2600 Castable Refractory
Pyrocast SC-2600 is a high purity silicon carbide based refractory for applications requiring high thermal conductivity, resistance to metal and flame abrasion.ApplicationsFilter boxes Burner tubes ..