Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 3.85e-7 - 0.000981 GPa @Temperature 110 °C, Time 86400 sec |
0.0000558 - 0.142 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories PT-165 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 3.85e-7 - 0.000981 GPa @Temperature 110 °C, Time 86400 sec |
0.0000558 - 0.142 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories PT-170 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 3.85e-7 - 0.000981 GPa @Temperature 110 °C, Time 86400 sec |
0.0000558 - 0.142 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories PTA-175 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 3.85e-7 - 0.000981 GPa @Temperature 110 °C, Time 86400 sec |
0.0000558 - 0.142 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories PTA-180 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 3.85e-7 - 0.000981 GPa @Temperature 110 °C, Time 86400 sec |
0.0000558 - 0.142 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories PTF-175 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 3.85e-7 - 0.000981 GPa @Temperature 110 °C, Time 86400 sec |
0.0000558 - 0.142 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories PTC-130S Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |