Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.01913 GPa @Temperature 1500 °C, Time 10800 sec |
2.775 ksi @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories A80 Special High-Density Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |