Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.0150 GPa @Temperature 1100 °C |
2.18 ksi @Temperature 2010 °F |
Hot |
Sharadaa Ceramics VELECRETE RC 101 Rodding Castables Description: The Rodding Castables offered by us are user friendly in nature and does not require high energy mixing machines and vibrators. Free flowing in nature, these castables are designed in c.. |
|||
Modulus of Rupture | 0.0150 GPa @Temperature 1000 °C |
2.18 ksi @Temperature 1830 °F |
Cold |
Sharadaa Ceramics VELECRETE RC 101 Rodding Castables Description: The Rodding Castables offered by us are user friendly in nature and does not require high energy mixing machines and vibrators. Free flowing in nature, these castables are designed in c.. |
|||
Modulus of Rupture | 0.0150 GPa @Temperature 1100 °C |
2.18 ksi @Temperature 2010 °F |
Hot |
Sharadaa Ceramics VELECRETE RC 103 Rodding Castables Description: The Rodding Castables offered by us are user friendly in nature and does not require high energy mixing machines and vibrators. Free flowing in nature, these castables are designed in c.. |