Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Rupture = 1.138 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Rupture 0.007848 GPa

@Temperature 110 °C,
Time 86400 sec
1.138 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories A70 Special High-Density Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.007848 GPa

@Temperature 500 °C,
Time 10800 sec
1.138 ksi

@Temperature 932 °F,
Time 3.00 hour
Chosun Refractories APC-100G Acid-proof Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.007848 GPa

@Temperature 500 °C,
Time 10800 sec
1.138 ksi

@Temperature 932 °F,
Time 3.00 hour
Chosun Refractories APC-120 Acid-proof Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.007848 GPa

@Temperature 500 °C,
Time 10800 sec
1.138 ksi

@Temperature 932 °F,
Time 3.00 hour
Chosun Refractories APC-50G Acid-proof Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.007848 GPa

@Temperature 1400 °C
1.138 ksi

@Temperature 2550 °F
Chosun Refractories CRAG-S04 Long Stopper
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.007848 GPa

@Temperature 110 °C,
Time 86400 sec
1.138 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories CTC-63TD Monolithic Refractories for Ladle and Tundish
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.007848 - 0.011772 GPa

@Temperature 1500 °C,
Time 10800 sec
1.138 - 1.7074 ksi

@Temperature 2730 °F,
Time 3.00 hour
Chosun Refractories HACT-180 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.007848 - 0.011772 GPa

@Temperature 1350 °C,
Time 10800 sec
1.138 - 1.7074 ksi

@Temperature 2460 °F,
Time 3.00 hour
Chosun Refractories HACT-180G High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.007848 - 0.010791 GPa

@Temperature 1350 °C,
Time 10800 sec
1.138 - 1.5651 ksi

@Temperature 2460 °F,
Time 3.00 hour
Chosun Refractories PTF-180 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.007848 GPa

@Temperature 1350 °C,
Time 10800 sec
1.138 ksi

@Temperature 2460 °F,
Time 3.00 hour
Chosun Refractories TCH-175S Torpedo Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.007848 GPa

@Temperature 1500 °C,
Time 10800 sec
1.138 ksi

@Temperature 2730 °F,
Time 3.00 hour
Chosun Refractories TCH-175SV Torpedo Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.007848 GPa

@Temperature 1350 °C,
Time 10800 sec
1.138 ksi

@Temperature 2460 °F,
Time 3.00 hour
Chosun Refractories TCH-175Y Torpedo Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Copyright © lookpolymers.com All Rights Reserved