Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00760 GPa @Temperature 1315 °C |
1.10 ksi @Temperature 2399 °F |
|
Pyrotek Pyrocast PCR Abrasion-Resistant Refractory Castable Pyrocast PCR is an abrasion resistant, thermal shock resistant castable. It is suitable to give exceptional resistance for conditions such as rapid heating or rapid cooling.ApplicationsCarbon anode.. |
|||
Modulus of Rupture | 0.00760 GPa @Temperature 104 °C |
1.10 ksi @Temperature 219 °F |
Dried; ASTM C268 |
BNZ Materials Blazecrete 2500 HS Dense Castable Blazecrete 2500 HSis a high-duty castable designed to withstand loads and resist normal abrasion and erosion at moderate temperatures to 2500°F (1371°C). Use with Blaz 2100 for a dual component li.. |
|||
Modulus of Rupture | 0.00760 GPa @Temperature 104 °C |
1.10 ksi @Temperature 219 °F |
Dried; ASTM C268 |
BNZ Materials Blazecrete 2300 ARG Dense Castable Blazecrete 2300 ARG is an alumina-silica castable with high strength and abrasion resistance. For service to 2300°F (1260°C). May be gunned or slap-troweled over Blaz 2000G to obtain a high streng.. |