Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00690 GPa @Treatment Temp. 649 °C |
1.00 ksi @Treatment Temp. 1200 °F |
|
Pyrotek Pyrocast AR Castable Refractory Pyrocast AR is a fused silica castable refractory inert to liquid aluminum and its alloys. It is a high strength material offering resistance to erosion and mechanical damage. Parts cast from Pyro.. |
|||
Modulus of Rupture | 0.00690 GPa @Temperature 1095 °C |
1.00 ksi @Temperature 2003 °F |
|
Pyrotek Pyrocast PCR Abrasion-Resistant Refractory Castable Pyrocast PCR is an abrasion resistant, thermal shock resistant castable. It is suitable to give exceptional resistance for conditions such as rapid heating or rapid cooling.ApplicationsCarbon anode.. |
|||
Modulus of Rupture | 0.00690 GPa @Temperature 1427 °C |
1.00 ksi @Temperature 2601 °F |
|
Pyrotek Valcor® G Pre-Cast Shapes ApplicationsBurner blocks Skimmer blocks Cover blocks Specialty blocks Plungers Stirrers Spouts Feeder tubes AdvantagesProven performance in molten glass contact applications Smooth surface finish d.. |
|||
Modulus of Rupture | 0.00689 GPa @Temperature 1450 °C |
1.00 ksi @Temperature 2640 °F |
|
Zircar Ceramics DAHP Dense Alumina Hearth Plate ZIRCAR Dense Alumina Hearth Plates are used for supporting loads in high temperature furnaces and other thermal process systems. These dense plates are made of fully sintered fine grain high purity .. |