Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.02943 GPa @Temperature 1000 °C, Time 10800 sec |
4.269 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories HSC-18SC Dense and High-Strength Castable, Superdense Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.02943 GPa @Temperature 250 °C |
4.269 ksi @Temperature 482 °F |
|
Chosun Refractories SB65S Bricks, Oxide Bonded SiC Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.02943 GPa @Temperature 1400 °C |
4.269 ksi @Temperature 2550 °F |
|
Chosun Refractories SB75 Bricks, Oxide Bonded SiC Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.02943 GPa @Temperature 250 °C |
4.269 ksi @Temperature 482 °F |
|
Chosun Refractories SB85S Bricks, Oxide Bonded SiC Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.02943 GPa @Temperature 250 °C |
4.269 ksi @Temperature 482 °F |
|
Chosun Refractories SB90S Bricks, Oxide Bonded SiC Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.02943 GPa @Temperature 250 °C |
4.269 ksi @Temperature 482 °F |
|
Chosun Refractories SBSN20 Nozzle Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |