Mechanical Properties Metric English Comments
Modulus of Rupture 0.0093195 GPa

@Temperature 110 °C,
Time 86400 sec
1.3517 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories A50 Special High-Density Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.0093195 GPa

@Temperature 110 °C,
Time 86400 sec
1.3517 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories C35 Special High-Density Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).