Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chosun Refractories C35 Special High-Density Gunning Castable

Category Ceramic , Oxide , Silicon Oxide
Manufacturer Chosun Refractories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories C35 Special High-Density Gunning Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 2.04 g/cc

@Temperature 1000 °C,
Time 10800 sec
0.0737 lb/in³

@Temperature 1830 °F,
Time 3.00 hour
2.08 g/cc

@Temperature 110 °C,
Time 86400 sec
0.0751 lb/in³

@Temperature 230 °F,
Time 24.0 hour
Porosity 16 %

@Temperature 110 °C,
Time 86400 sec
16 %

@Temperature 230 °F,
Time 24.0 hour
20.5 %

@Temperature 1000 °C,
Time 10800 sec
20.5 %

@Temperature 1830 °F,
Time 3.00 hour
Mechanical Properties Metric English Comments
Modulus of Rupture 0.0093195 GPa

@Temperature 110 °C,
Time 86400 sec
1.3517 ksi

@Temperature 230 °F,
Time 24.0 hour
0.00981 GPa

@Temperature 1000 °C,
Time 10800 sec
1.42 ksi

@Temperature 1830 °F,
Time 3.00 hour
Thermal Properties Metric English Comments
Shrinkage -0.200 %

@Temperature 1000 °C,
Time 10800 sec
-0.200 %

@Temperature 1830 °F,
Time 3.00 hour
-0.100 %

@Temperature 110 °C,
Time 86400 sec
-0.100 %

@Temperature 230 °F,
Time 24.0 hour
Component Elements Properties Metric English Comments
Al2O3 35 %
35 %
SiO2 55 %
55 %
Descriptive Properties Value Comments
Main Applications General furnace
Material Required for Estimating (kg/?) 2,050