Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00207 GPa @Temperature 1371 °C |
0.300 ksi @Temperature 2500 °F |
ASTM C268 |
BNZ Materials Bazelite 2600 LI Insulating Castable Blaz 2600 LI is s low iron, high purity castable for service to 2600°F (1427°C) in controlled atmosphere applications. Recommended for casting monolithic shapes and furnace liningsInformation prov.. |