Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00165 GPa @Temperature 104 °C |
0.239 ksi @Temperature 219 °F |
Dried; ASTM C268 |
BNZ Materials Bazelite 2600 LI Insulating Castable Blaz 2600 LI is s low iron, high purity castable for service to 2600°F (1427°C) in controlled atmosphere applications. Recommended for casting monolithic shapes and furnace liningsInformation prov.. |