Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00140 GPa @Temperature 1095 °C |
0.203 ksi @Temperature 2003 °F |
ASTM C268 |
BNZ Materials Blazecrete 2500 HS Dense Castable Blazecrete 2500 HSis a high-duty castable designed to withstand loads and resist normal abrasion and erosion at moderate temperatures to 2500°F (1371°C). Use with Blaz 2100 for a dual component li.. |
|||
Modulus of Rupture | 0.00140 GPa @Temperature 1095 °C |
0.203 ksi @Temperature 2003 °F |
ASTM C268 |
BNZ Materials Blazecrete 2300 ARG Dense Castable Blazecrete 2300 ARG is an alumina-silica castable with high strength and abrasion resistance. For service to 2300°F (1260°C). May be gunned or slap-troweled over Blaz 2000G to obtain a high streng.. |