Mechanical Properties Metric English Comments
Ultimate Bearing Strength 349 MPa
50600 psi
Average value longitudinal with bearing strain 8.9%.
Materion AlBeMet® AM 162 Extruded Bar, Annealed
Mechanical property values below are in the longitudinal direction; transverse values generally lower. This is a powder metallurgical product produced by gas atomization available as rod, bar, tube..